Description: GSE-48 Thermoplastic Elastomer Modifier, developing for seamlessly blending with EVA and PE to replace the original function of synthetic rubbers in its place of formulated mixture in DCP crosslink foaming method. GSE-48 has same effect and properties as those of synthetic rubbers, where GSE-48 not only modify and improve the mixture but exceed the desired effect of synthetic rubbers to creat more value for your products.
Form: | Pellet |
Color: | Natural (white) |
Packing: | 25 kg /Bag |
Property |
Unit |
Standard |
Value |
g/10min |
ASTM D1238 |
0.1~1.0 |
|
Density |
g/cm3 |
ASTM D792 |
0.95~1.05 |
Hardness |
Shore A |
ASTM D2240 |
46±2 |
Tensile Strength |
kg/cm2 |
ASTM D412 |
25 |
Elongation |
% |
ASTM D412 |
1081 |
Tear Strength |
kg/cm |
ASTM D624 |
18 |
Softening Point |
oC |
ASTM D1525 |
60-65 |
Feature:
Applicable to your original formula by replacing the intended place of synthetic rubbers such as IR, EPDM, BR, SBR and POE in equal volume with GSE-48. With application of GSE-48, you will not only to have better result comparing to synthetic rubber but to save cost on cutting, mastication and storage.
SGS certified of PAHs & 14P free (Report No. TE/2014/70099R1)